Atomic Layer Deposition of Nanostructured Materials (eBook)

Nicola Pinna, Mato Knez (Herausgeber)

eBook Download: PDF
2012 | 1. Auflage
XXXVI, 436 Seiten
Wiley-VCH (Verlag)
978-3-527-63993-9 (ISBN)

Lese- und Medienproben

Atomic Layer Deposition of Nanostructured Materials -
Systemvoraussetzungen
156,99 inkl. MwSt
  • Download sofort lieferbar
  • Zahlungsarten anzeigen
Atomic layer deposition, formerly called atomic layer epitaxy, was developed in the 1970s to meet the needs of producing high-quality, large-area fl at displays with perfect structure and process controllability. Nowadays, creating nanomaterials and producing nanostructures with structural perfection is an important goal for many applications in nanotechnology. As ALD is one of the important techniques which offers good control over the surface structures created, it is more and more in the focus of scientists. The book is structured in such a way to fi t both the need of the expert reader (due to the systematic presentation of the results at the forefront of the technique and their applications) and the ones of students and newcomers to the fi eld (through the first part detailing the basic aspects of the technique).

This book is a must-have for all Materials Scientists, Surface Chemists, Physicists, and Scientists in the Semiconductor Industry.

Nicola Pinna studied physical chemistry at the Université Pierre et Marie Curie (Paris). He received his PhD in 2001, and in 2002, he moved to the Fritz Haber Institute of the Max Planck Society (Berlin). In 2003, he joined the Max Planck Institute of Colloids and Interfaces (Potsdam). In 2005, he moved to the Martin Luther University, Halle-Wittenberg, as an Assistant Professor of Inorganic Chemistry. Since 2006 he is researcher at the Department of Chemistry and CICECO of the University of Aveiro and since 2009 he is also Assistant Professor at the School of Chemical and Biological Engineering of the Seoul National University. In 2011 he was ranked among the top 100 materials scientists of the past decade by impact. His research activity is focused on the development of novel routes to nanostructured materials, their characterization, and the study of their physical properties. Mato Knez studied chemistry at the University of Ulm in Germany. He did his dissertation at the Max Planck Institute of solid state research in Stuttgart from 2000-2003. In 2003 he joined the Max Planck Institute for Microstructure Physics in Halle as a Postdoc where he established the ALD-based research direction. Since 2006 he is leading a research group funded by the German Ministry of Education and Research (BMBF). In January 2012 he will join CIC nanoGUNE in San Sebastian (Spain) as an Ikerbasque Research Professor. His research activities are mainly focused on various aspects of the application of ALD, including the synthesis of optical nanolaminates, infi ltration mechanisms when ALD is applied to soft materials, and ALD-assisted nanofabrication of photonic and plasmonic structures. Aside from ALD he has strong research activites in biotemplated inorganic nanostructures for applications in nanotechnology and medicine.

PART I: Introduction to ALD

THEORETICAL MODELING OF ALD PROCESSES
Introduction
Overview of Atomistic Simulations
Calculation of Properties Using Quantum Simulations
Prediction of ALD Chemical Mechanisms
Example of a Calculated ALD Mechanism: ALD of Al2O3 Using TMA and Water

STEP COVERAGE IN ALD
Introduction
Growth Techniques
Step Coverage Models in ALD
Experimental Verifications of Step Coverage Models
Summary

PRECURSORS FOR ALD PROCESSES
Introduction
General Requirements for ALD Precursors
Metallic Precursors for ALD
Nonmetal Precursors for ALD
Conclusions

SOL-GEL CHEMSTRY AND ATOMIC LAYER DEPOSITION
Aqueous and Nonaqueous Sol-Gel in Solution
Sol-Gel and ALD: An Overview
Mechanistic and In Situ Studies

MOLECULAR LAYER DEPOSITION OF HYBRID ORGANIC-INORGANIC FILMS
Introduction
General Issues for MLD of Hybrid Organic-Inorganic Films
MLD Using Trimethylaluminum and Ethylene Glycol in an AB Process
Expansion to an ABC Process Using Heterobifunctional and Ring-Opening Precursors
Use of a Homotrifunctional Precursor to Promote Cross-Linking in an AB Process
MLD of Hybrid Alumina-Siloxane Films Using an ABCD Process
Future Prospects for MLD of Hybrid Organic-Inorganic Films´

LOW-TEMPERATURE ATOMIC LAYER DEPOSITION
Introduction
Challenges of LT-ALD
Materials and Processes
Toward Novel LT-ALD Processes
Thin Film Gas Diffusion Barriers
Encapsulation of Organic Electronics
Conclusions

PLASMA ATOMIC LAYER DEPOSITION
Introduction
Plasma Basics
Plasma ALD Configurations
Merits of Plasma ALD
Challenges for Plasma ALD
Concluding Remarks and Outlook

PART II: Nanostructures by ALD

ATOMIC LAYER DEPOSITION FOR MICROELECTRONIC APPLICATIONS
Introduction
ALD Layers for Memory Devices
ALD for Logic Devices
Concluding Remarks

NANOPATTERNING BY AREA-SELECTIVE ATOMIC LAYER DEPOSITION
Concept of Area-Selective Atomic Layer Deposition
Change of Surface Properties
Patterning
Applications of AS-ALD
Current Challenges

COATINGS ON HIGH ASPECT RATIO STRUCTURES
Introduction
Models and Analysis
Characterization Methods for ALD Coatings in High Aspect Ratio Structures
Examples of ALD in High Aspect Ratio Structures
Nonideal Behavior during ALD in High Aspect Ratios
Conclusions and Future Outlook

COATINGS OF NANOPARTICLES AND NANOWIRES
ALD on Nanoparticles
Vapor-Liquid-Solid Growth of Nanowires by ALD
Atomic Layer Epitaxy on Nanowires
ALD on Semiconductor NWs for Surface Passivation
ALD-Assisted Formation of Nanopeapods
Photocorrosion of Semiconductor Nanowires Capped by ALD Shell
Interface Reaction of Nanowires with ALD Shell
ALD ZnO on NWs/Tubes as Seed Layer for Growth of Hyperbranch
Conclusions

ATOMIC LAYER DEPOSITION ON SOFT MATERIALS
Introduction
ALD on Polymers for Passivation, Encapsulation, and Surface Modification
ALD for Bulk Modification of Natural and Synthetic Polymers and Molecules
ALD for Polymer Sacrificial Templating: Membranes, Fibers, and Biological and Optical Structures
ALD Nucleation of Patterned and Planar SAMs and Surface Oligomers
Reactions during Al2O3 ALD on Representative Polymer Materials
Summary

APPLICATION OF ALD TO BIOMATERIALS AND BIOCOMPATIBLE COATINGS
Application of ALD to Biomaterials
Biocompatible Coatings
Summary

COATING OF CARBON NANOTUBES
Introduction
Purification and Surface Functionalization of Carbon Nanotubes
Decoration/Coating of Carbon Nanotubes by Solution Routes
Decoration/Coating of Carbon Nanotubes by Gas-Phase Techniques
Atomic Layer Deposition on Carbon Nanotubes
Coating of Large Quantity of CNTs by ALD
ALD Coating of Other sp2-Bonded Carbon Materials
Conclusions

INVERSE OPAL PHOTONICS
Introduction and Background
Properties of Three-Dimensional Photonic Band Structures
Large-Pore and Non-Close-Packed Inverse Opals
Experimental Studies
Tunable PC Structures
Summary

NANOLAMINATES
Introduction
Optical Applications
Thin Film Encapsulation
Applications in Electronics
Copper Electroplating Applications
Solid Oxide Fuel Cells
Complex Nanostructures
Summary

CHALLENGES IN ATOMIC LAYER DEPOSITION
Introd

Erscheint lt. Verlag 19.9.2012
Sprache englisch
Themenwelt Naturwissenschaften Chemie
Technik
Schlagworte Analyse u. Charakterisierung von Nanosystemen • Analysis/Characterization of Nanosystems • Atomlagenabscheidung • Dünne Schicht • Dünne Schichten, Oberflächen u. Grenzflächen • Dünne Schicht • Dünne Schichten, Oberflächen u. Grenzflächen • Electrical & Electronics Engineering • Electronic materials • Elektronische Materialien • Elektrotechnik u. Elektronik • Materials Science • Materialwissenschaften • Nanomaterial • Nanomaterialien • nanomaterials • Nanostrukturiertes Material • Nanotechnologie • nanotechnology • Sensoren • Sensor Materials • Synthese u. Produktion von Nanosystemen • Synthesis/Production of Nanosystems • Thin Films, Surfaces & Interfaces
ISBN-10 3-527-63993-4 / 3527639934
ISBN-13 978-3-527-63993-9 / 9783527639939
Haben Sie eine Frage zum Produkt?
PDFPDF (Adobe DRM)
Größe: 8,4 MB

Kopierschutz: Adobe-DRM
Adobe-DRM ist ein Kopierschutz, der das eBook vor Mißbrauch schützen soll. Dabei wird das eBook bereits beim Download auf Ihre persönliche Adobe-ID autorisiert. Lesen können Sie das eBook dann nur auf den Geräten, welche ebenfalls auf Ihre Adobe-ID registriert sind.
Details zum Adobe-DRM

Dateiformat: PDF (Portable Document Format)
Mit einem festen Seiten­layout eignet sich die PDF besonders für Fach­bücher mit Spalten, Tabellen und Abbild­ungen. Eine PDF kann auf fast allen Geräten ange­zeigt werden, ist aber für kleine Displays (Smart­phone, eReader) nur einge­schränkt geeignet.

Systemvoraussetzungen:
PC/Mac: Mit einem PC oder Mac können Sie dieses eBook lesen. Sie benötigen eine Adobe-ID und die Software Adobe Digital Editions (kostenlos). Von der Benutzung der OverDrive Media Console raten wir Ihnen ab. Erfahrungsgemäß treten hier gehäuft Probleme mit dem Adobe DRM auf.
eReader: Dieses eBook kann mit (fast) allen eBook-Readern gelesen werden. Mit dem amazon-Kindle ist es aber nicht kompatibel.
Smartphone/Tablet: Egal ob Apple oder Android, dieses eBook können Sie lesen. Sie benötigen eine Adobe-ID sowie eine kostenlose App.
Geräteliste und zusätzliche Hinweise

Zusätzliches Feature: Online Lesen
Dieses eBook können Sie zusätzlich zum Download auch online im Webbrowser lesen.

Buying eBooks from abroad
For tax law reasons we can sell eBooks just within Germany and Switzerland. Regrettably we cannot fulfill eBook-orders from other countries.

Mehr entdecken
aus dem Bereich
Eigenschaften, Verarbeitung, Konstruktion

von Erwin Baur; Dietmar Drummer; Tim A. Osswald …

eBook Download (2022)
Carl Hanser Fachbuchverlag
53,99