Surface Analysis for High Efficiency Silicon Solar Cells
Seiten
2017
Fraunhofer Verlag
978-3-8396-1117-3 (ISBN)
Fraunhofer Verlag
978-3-8396-1117-3 (ISBN)
In the case of silicon solar cells the desire for higher efficiencies leads to technological improvements. This thesis addresses the impact of physical properties of wet-chemically treated silicon surfaces on the solar cell characteristics. The distinct knowledge about the surface characteristics is found to be a key factor to improve highly efficient silicon solar cells even further.
Erscheinungsdatum | 08.02.2017 |
---|---|
Reihe/Serie | Solare Energie- und Systemforschung / Solar Energy and Systems Research |
Zusatzinfo | num., mostly col. illus. and tab. |
Verlagsort | Stuttgart |
Sprache | englisch |
Maße | 148 x 210 mm |
Themenwelt | Naturwissenschaften ► Physik / Astronomie ► Festkörperphysik |
Technik ► Elektrotechnik / Energietechnik | |
Technik ► Maschinenbau | |
Schlagworte | Alternative & renewable energy sources & technolog • Aluminiumoxid • Condensed matter physics (liquid state & solid sta • condensed matter physics (liquid state & solid state physics) • Festkörperphysik • Fraunhofer ISE • Materials Science • Materialwissenschaftler • Nasschemische Vorbehandlung • Oberflächenphysik • Physiker • Siliziumsolarzellen • Technologen |
ISBN-10 | 3-8396-1117-2 / 3839611172 |
ISBN-13 | 978-3-8396-1117-3 / 9783839611173 |
Zustand | Neuware |
Haben Sie eine Frage zum Produkt? |
Mehr entdecken
aus dem Bereich
aus dem Bereich
Aufgaben und Lösungen
Buch | Softcover (2023)
De Gruyter Oldenbourg (Verlag)
39,95 €