Progress on Pellet–Cladding Interaction and Stress Corrosion Cracking
Experimentation, Modelling and Methodologies Applied to Support the Flexible Operation of Nuclear Power Plants: Report of a Technical Meeting
Seiten
2021
IAEA (Verlag)
978-92-0-116521-3 (ISBN)
IAEA (Verlag)
978-92-0-116521-3 (ISBN)
Provides an overview of pellet-cladding interaction/stress corrosion cracking (PCI/SCC) and reports on the progress made since the early 2000s, based on presentations and discussions at a related IAEA technical meeting held in October 2019.
Flexible operation and related power changes can have a direct impact on fuel integrity through pellet–cladding interaction/stress corrosion cracking (PCI/SCC) phenomena, which could lead to fuel failures in certain conditions. For some anticipated operational occurrences that affect fuel with small PCI/SCC margins, the fuel failures caused by PCI/SCC cannot be assumed to be benign, and a significant radiological source term may be generated. This publication provides an overview of PCI/SCC studies and reports on the progress made since the early 2000s, based on presentations and discussions at a related IAEA technical meeting held in October 2019.
Flexible operation and related power changes can have a direct impact on fuel integrity through pellet–cladding interaction/stress corrosion cracking (PCI/SCC) phenomena, which could lead to fuel failures in certain conditions. For some anticipated operational occurrences that affect fuel with small PCI/SCC margins, the fuel failures caused by PCI/SCC cannot be assumed to be benign, and a significant radiological source term may be generated. This publication provides an overview of PCI/SCC studies and reports on the progress made since the early 2000s, based on presentations and discussions at a related IAEA technical meeting held in October 2019.
Erscheinungsdatum | 04.02.2022 |
---|---|
Reihe/Serie | IAEA TECDOC |
Zusatzinfo | 13 illustrations |
Verlagsort | Vienna |
Sprache | englisch |
Maße | 210 x 297 mm |
Gewicht | 830 g |
Themenwelt | Naturwissenschaften ► Physik / Astronomie ► Atom- / Kern- / Molekularphysik |
Technik ► Elektrotechnik / Energietechnik | |
ISBN-10 | 92-0-116521-8 / 9201165218 |
ISBN-13 | 978-92-0-116521-3 / 9789201165213 |
Zustand | Neuware |
Haben Sie eine Frage zum Produkt? |
Mehr entdecken
aus dem Bereich
aus dem Bereich
Buch | Softcover (2024)
Wiley-VCH (Verlag)
59,90 €